Secant Modulus, MD 0.655 GPa
95.0 ksi
Film; 1% secant; ASTM D882A
LyondellBasell Pro-fax SA861 Polypropylene Random Copolymer, Cast Film Extrusion
Key Features: polypropylene random copolymer resin formulated for cast film extrusion, good optical properties, excellent slip properties, FDA acceptable, improved cold temperature impact resistance..