Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.062563 GPa | 9.0741 ksi | 2% Secant; ASTM D882 |
Dow ATTANE™ 4404G, 2mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G provides improved cling in one-sided cling applications, and has improved toughness and optical properties. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information provided by.. |