Polymer Property : Secant Modulus, MD = 564.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 2.758 - 3.889 GPa
400.0 - 564.1 ksi
ASTM D882
Honeywell Capran® Emblem™ 1000 Bi-Axially Oriented Nylon 6 Film
Description: Capran® Emblem™ 1000 is a 0.40 mil (10 micron) biaxially oriented nylon 5 film with excellent flex crack resistance and superior clarity properties. Applications: packaging appl..