Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.385 GPa | 55.8 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® TF-0242-E Hexene LLDPE Film Resin
(discontinued **) Excellent stiffness and glossApplications: Diaper back sheet, BlendingFilm properties are typical of film extruded at 270°C.Information provided by NOVA Chemicals. |