Polymer Property : Secant Modulus, MD = 41.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.289 GPa
41.9 ksi
2% Secant; ASTM D882
Dow INTEGRALâ„¢ 932 High Heat Multilayer Adhesive Film
INTEGRAL 925 High Heat Adhesive Film is a heat-activated, thermally stable adhesive film for automotive applications capable of bonding to urethane foam-baked fabrics, paper, fiberglass, non-wovens,..