Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.2682 GPa | 38.90 ksi | 2% Secant; ASTM D882 |
Dow DOWLEX™ 2071D Linear Low Density Polyethylene Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |