Polymer Property : Secant Modulus, MD = 33.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.234 GPa
33.9 ksi
0.01; ASTM D882
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services  (discontinued *
VORIDIAN HIFOR CLEAR SC74558-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives. Films produced with t..
Secant Modulus, MD 0.234 GPa
33.9 ksi
1% Secant; ASTM D882
Westlake Hifor SC74560-F Clear Polyethylene  (discontinued **)
Hifor Clear Polyethylene SC74560-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and medium antiblock additives. Films produc..