Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.214 GPa | 31.0 ksi | Value at 0.1 mm/mm-min Initial Strain Rate; ASTM D882 |
Bapolene® 122F Polyethylene, Film Grade Bapolene LL122F is a general purpose LLDPE for blown film extrusion applications. This resin offers excellent tensile and toughness properties. Contains medium levels of slip/antiblock additives. .. |
|||
Secant Modulus, MD | 0.214 GPa | 31.0 ksi | ASTM D882 |
ExxonMobil Escorene® LL-3218 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3218 have outstanding tensile properties as well as stiffness and toughness. These su.. |