Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 2.08 GPa | 301 ksi | ASTM D822 |
DuPont™ Tedlar® TTR10BG3 Transparent Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |