Mechanical Properties Metric English Comments
Secant Modulus, MD 1.76 - 9.12 GPa
256 - 1320 ksi
Average value: 5.34 GPa Grade Count:3
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..