Mechanical Properties Metric English Comments
Secant Modulus, MD 0.173 GPa
25.1 ksi
ASTM D882
Huntsman PE 1011 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good impact strength, good machinability, heat seal and foaming characteristicsApplications: Film Extrusion: industrial line..
Secant Modulus, MD 0.173 GPa
25.1 ksi
ASTM D882
Huntsman PE1020 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Medium impact strength and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 ..
Secant Modulus, MD 0.173 GPa
25.1 ksi
ASTM D882
Huntsman PE1041 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Good optical, medium impact strength, and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 2..
Secant Modulus, MD 0.173 GPa
25.1 ksi
ASTM D882
Huntsman PE1058 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional draw down and processability, excellent strength, good heat sealability, and optics.Applications: Film extrusion: all thin film uses and especiall..