Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.0496 - 0.165 GPa | 7.20 - 23.9 ksi | Average value: 0.108 GPa Grade Count:7 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m.. |