Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.164 GPa | 23.8 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® LA-0424-A LDPE Foam Resin Good stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film extr.. |