Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus, MD = 21.38 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.1474 GPa
21.38 ksi
2% Secant; ASTM D882
Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin
Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-1003 NT 7 is an ethylene-hexene-1 copolymer, design..