Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.0300 - 1.40 GPa | 4.35 - 203 ksi | Average value: 0.841 GPa Grade Count:85 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |