Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.0830 - 1.28 GPa | 12.0 - 185 ksi | Average value: 0.232 GPa Grade Count:19 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |