Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.128 GPa | 18.6 ksi | 2% Secant; ASTM D882 |
Dow ATTANE™ 4201G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G is used for packaging applications. It offers toughness, seal properties, optical properties and processability. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information prov.. |
|||
Secant Modulus, MD | 0.128 GPa | 18.6 ksi | ASTM D882 |
Huntsman PE1403 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA Copolymer, DMF listed and FDA compliantFeatures: High clarity film with good toughness and flexibility at low temperatures.Applications: Film extrusion: frozen food and general .. |