Polymer Property : Secant Modulus, MD = 1.80 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 1.80 GPa
261 ksi
0.01; ASTM D882
Eastman Sahara Film
Sahara Films are developed for use in applications where increased temperature resistance is desired.Applications/UsesHigh temperature printable films