Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.696 - 1.32 GPa | 101 - 191 ksi | Average value: 1.04 GPa Grade Count:7 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |