Polymer Property : Secant Modulus, MD = 1.275 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 1.275 GPa
184.9 ksi
at 1%; ASTM D882
Chevron Phillips K-Resin® KR10 Styrene-Butadiene Copolymer, Film Grade  (discontinued **)
Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: This SBC is easily processed on blown film or cast fi..