Secant Modulus, MD 1.237 GPa
179.4 ksi
ASTM D882
ExxonMobil Escorene® HD-7745 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7745 exhibit excellent impact and toughness properties as well as high stiffness...