Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.835 GPa | 121 ksi | ASTM Test |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |