Mechanical Properties Metric English Comments
Secant Modulus, MD 0.800 GPa
116 ksi
ASTM D882
SCG Chemicals EL-Leneâ„¢ H5604F High Density Polyethylene Film
Key Characteristics:High tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierRecommended Applications: Films for shopping bag, T-shirt bag, garbage bag, liner bagInfor..