Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.470 GPa | 68.2 ksi | |
UBE 1022FDX29 Nylon 6 Homopolymer Film Specialties: Nucleated (Medium viscosity) Processing: T-die, Air blown Applications: General applications Information provided by UBE. |