Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.469 GPa | 68.0 ksi | ASTM D882 |
Honeywell Stretch-Vac® 2000 Heat-Stabilized Blown Film
(discontinued **) Description: Stretch-Vac® 2000 is a pink tinted, high elongation, heat-stabilized blown film produced from modified polyamide resin. It is available in widths up to 80 inches as layflat tubing and.. |
|||
Secant Modulus, MD | 0.469 GPa | 68.0 ksi | ASTM D882 |
Honeywell Stretch-Vac® Elastomax 1000 Heat-Stabilized Blown Film
(discontinued **) Description: Capran® Elastomax 1000 is a pink tinted, heat-stabilized blown film produced from modified nylon resin. It is available in widths up to 80 inches as layflat tubing and 120 inches as s.. |