Polymer Property : Secant Modulus, MD = 0.450 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.450 GPa
65.3 ksi
ASTM D882
Chevron Phillips HiD® 9640 HDPE Blown Film Resin  (discontinued **)
Copolymerization Enhances Film Toughness, Unique Combination of Density and Melt Index, Excellent Strength Properties as well as Good Heat Seal, Lower Density Imparts a Softer Feel and Lesser Tenden..