Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.116 - 0.230 GPa | 16.8 - 33.4 ksi | Average value: 0.171 GPa Grade Count:33 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum.. |