Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.185 GPa | 26.8 ksi | 1%; ASTM D882 |
Braskem LF 0720/21 AF LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); high clarity films; "liners"; general purpose. Information provided by Braskem |