Mechanical Properties Metric English Comments
Secant Modulus, MD 0.1809 GPa
26.23 ksi
2% Secant; ASTM D882
Dow ELITE™ 5401G Enhanced Polyethylene Resin
™ 5401G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of low seal initiation, moderate stiffness and low blocking for excellent performance on a..