Mechanical Properties Metric English Comments
Secant Modulus, MD 0.1494 GPa
21.67 ksi
2% Secant; ASTM D882
Dow DOWLEX™ 2267G Linear Low Density Polyethylene
A high performance stretch film resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow