Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.125 GPa | 18.1 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding.. |
|||
Secant Modulus, MD | 0.125 GPa | 18.1 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity,.. |