Mechanical Properties Metric English Comments
Secant Modulus, MD 0.124 GPa
18.0 ksi
ASTM D882
ExxonMobil Escorene® LD-317 EVA Film Resin, FMI  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 5.5% vinyl acetate copolymer film resin. Film made from LD-317 offers excellent impact strength, tensile properties, and h..
Secant Modulus, MD 0.124 GPa
18.0 ksi
ASTM D882
Huntsman PE1407 EVA Film Extrusion  (discontinued **)
4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Secant Modulus, MD 0.124 GPa
18.0 ksi
50 µm (2 mil) film; ASTM D882
DuPont Nucrel® 31001 Ethylene-Acrylic Acid Copolymer Resin for Blown and Cast Film
9.5 wt% Acrylic Acid.Nucrel® 31001 is an ethylene-acrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.F..
Secant Modulus, MD 0.124 GPa
18.0 ksi
ASTM D882
Huntsman Rexell® L3102 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Good impact and puncture resistance with excellent optics and sealability.Applications: Laminated and coextruded films for ..