Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.0930 GPa | 13.5 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend The Trilene TS 8056 product is a blend with a high ratio of linear low-density polyethylene - octene comonomer (LLDPE-C8) with low-density polyethylene (LDPE) with elevated processability, ensuring .. |
|||
Secant Modulus, MD | 0.0930 GPa | 13.5 ksi | ASTM D882 |
Huntsman PE1903 EVA Film Extrusion
(discontinued **) 9% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent toughness and flexibility at low temperatures, and good heat-seal response.Applications: Film extrusion: laminating film, controll.. |