Polymer Property : Shear Strength = 9990 psi
Polymer Property :
Shear Strength =
9990 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Shear Strength
68.9
MPa
9990
psi
Compression interlaminar; RT
Hexcel® HexPly® F155 Epoxy Resin, 181 Glass Fabric
Information provided by HexCel