Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 97.2 MPa | 14100 psi | Ultimate; ASTM D3846 |
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK) Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent .. |
|||
Shear Strength | 97.2 MPa | 14100 psi | Ultimate; ASTM D3846 |
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK) Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent fle.. |
|||
Shear Strength | 97.2 MPa @Temperature 22.8 °C |
14100 psi @Temperature 73.0 °F |
Ultimate; ASTM D3846 |
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |