Polymer Property : Shear Strength = 96.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 49.6 - 96.0 MPa
7190 - 13900 psi
Average value: 80.6 MPa Grade Count:10
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..