Polymer Property : Shear Strength = 93.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 93.8 MPa

@Temperature 23.9 °C
13600 psi

@Temperature 75.0 °F
Short-Beam, Dry; ASTM D2344
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen..