Mechanical Properties Metric English Comments
Shear Strength 80.8 - 89.0 MPa
11700 - 12900 psi
Average value: 84.3 MPa Grade Count:5
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..