Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 88.3 MPa @Thickness 15.7 mm |
12800 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP630 Paper Base Laminate Description: Machining grade with good electrical properties and moisture resistance. Low cold flow with good dimensional stability. Thickness Tested: 0.062", 0.125", and 0.500" |