Shear Strength >= 5.62 MPa
>= 815 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRP - 3/16 - 12.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength 5.62 MPa
815 psi
Overlap, Isopropyl Alcohol Wipe surface prep, PVC
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..