Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 8.89 MPa | 1290 psi | Overlap, PC/ABS Alloy / PC/ABS Alloy; ASTM D1002 |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 8.89 MPa | 1290 psi | Overlap, PC/ABS Alloy / PC/ABS Alloy; ASTM D1002 |
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |