Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 5.38 MPa | 780 psi | |
Valley Adhesives EM-115 High Performance Application Glue Stick Valley Adhesives EM-115 High Performance Application Glue StickHigh peel, shear strength, and heat resistance; Good wetting and heat resistance for potting; Excellent adhesion to wood, plastics, pol.. |