Polymer Property : Shear Strength = 74.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 74.5 MPa
10800 psi
ASTM D732
Network Polymers Kepital® F20-25
Description: Natural Acetal Copolymer, 25% Glass Reinforced GradeInformation provided by Network Polymers Inc.
Shear Strength 74.5 MPa

@Temperature 23.0 °C
10800 psi

@Temperature 73.4 °F
ASTM D732
DuPont Performance Polymers Rynite® 830ER NC010 PET
Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers