Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 4.90 MPa | 710 psi | Lap; ASTM 1002 |
Arlon Thermabond® 48991A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation IIa Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style .. |