Polymer Property : Shear Strength = 7000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 48.3 - 55.2 MPa
7000 - 8000 psi
ASTM D732
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Shear Strength 48.3 - 62.1 MPa
7000 - 9000 psi
ASTM D732
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Shear Strength 48.3 - 55.2 MPa
7000 - 8000 psi
ASTM D732
Mar-Bal MB5500 Thermoset Polyester Composite Molding Compound
A superior heat resistant material. U.L. RTI rating of 160°C-170°C.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Shear Strength 48.3 MPa

@Temperature 25.0 °C
7000 psi

@Temperature 77.0 °F
Die
Lord Adhesives Thermosetâ„¢ MD-110 Conductive Adhesive
LORD Thermosetâ„¢ MD-110 silver-filled conductive adhesive offers excellent electrical conductivity and room temperature stability. It is designed for use with automated dispensing, stamping and..
Shear Strength 48.3 MPa

@Temperature 25.0 °C
7000 psi

@Temperature 77.0 °F
Die
Lord Adhesives Thermosetâ„¢ MD-140 Conductive Adhesive
LORD Thermosetâ„¢ MD-140 silver-filled conductive adhesive offers excellent thermal conductivity. It is designed for use in thermally demanding die attach applications such as microprocessor, po..