Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.476 MPa | 69.0 psi | Cohesion Dynamic, PET/Polycarbonate; ASTM D1002 |
3M 7959MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Shear Strength | 0.476 MPa | 69.0 psi | Overlap, Pine, 50% RH |
3M PN8017 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Shear Strength | 0.476 MPa | 69.0 psi | Overlap, Pine, 50% RH |
3M PN8019 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Shear Strength | 0.476 MPa | 69.0 psi | Overlap, Pine, 50% RH |
3M PN8027 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Shear Strength | 0.476 MPa | 69.0 psi | Cohesion Dynamic, PET/Polycarbonate; ASTM D1002 |
3M 9059MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Shear Strength | 0.476 MPa | 69.0 psi | Overlap, Pine, 50% RH |
3M PN8029 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |