Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 47.4 MPa | 6870 psi | |
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Injection Grade Durez 32633 Black Phenolic is a two-stage, glass filled, special purpose molding compound. It is designed for applications requiring high physical strengths, dimensional stability, and heat resista.. |