Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.455 MPa | 66.0 psi | Overlap, Polypropylene, 50% RH |
3M 5200 Marine Adhesive/Sealant Fast Cure A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds with excellent adhesion to wood and fiberglass. Forms watertight, weather-resistant seals .. |
|||
Shear Strength | 0.455 MPa | 66.0 psi | Cohesion Dynamic, PET/Polycarbonate; ASTM D1002 |
3M 7957MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Shear Strength | 0.455 MPa | 66.0 psi | Cohesion Dynamic, PET/Polycarbonate; ASTM D1002 |
3M 7961MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Shear Strength | 0.455 MPa | 66.0 psi | Cohesion Dynamic, PET/Polycarbonate; ASTM D1002 |
3M 9061MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Shear Strength | 0.455 MPa | 66.0 psi | Cohesion Dynamic, PET/Polycarbonate; ASTM D1002 |
3M 9057MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |