Polymer Property : Shear Strength = 59.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 59.3 MPa

@Temperature 21.1 °C
8600 psi

@Temperature 70.0 °F
Short-Beam, Dry; ASTM D2344
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 6781 S2-Glass
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Shear Strength 59.3 MPa

@Temperature 23.9 °C
8600 psi

@Temperature 75.0 °F
Short-Beam, Dry; ASTM D2344
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f..