Shear Strength >= 0.393 MPa
>= 57.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® CR III 1/4-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength >= 0.393 MPa
>= 57.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® CR III 3/8-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength >= 0.393 MPa
>= 57.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength >= 0.393 MPa
>= 57.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 0.393 MPa
57.0 psi
Cold Rolled Steel, after 48 hrs at 23°C
3M Fastbond™ 49 Insulation Adhesive
3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and ..
Shear Strength 0.393 MPa
57.0 psi
Polycarbonate, after 48 hrs at 23°C
3M Fastbond™ 49 Insulation Adhesive
3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and ..
Shear Strength 0.393 MPa
57.0 psi
Overlap, Fir, 50% RH
3M PN8017 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Shear Strength 0.393 MPa
57.0 psi
Overlap, Fir, 50% RH
3M PN8019 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Shear Strength 0.393 MPa
57.0 psi
Overlap, Fir, 50% RH
3M PN8027 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Shear Strength 0.393 MPa
57.0 psi
Overlap, Fir, 50% RH
3M PN8029 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..